Powder Coating News
now browsing by category
Hot news ,developing ,technology of powder coating industry .
Installation of spray booths
The powder supply and coating powder feedlines should be interlocked with the air extraction system,so that ,in the event of failure of the ventilatioon system,the coating powder and powder supplies are cut off.Airflow monitor switches are the preferred method of detecting failure of the ventilation system.Such equipment will also be sensitive to blocked filters and broken or loose fan blades. A fire detecting device,interlocked to shut off powder and coating powder supplies and ventilation may be installed in the boothRead More …
Location of stoving ovens
The stoving oven should be situated at least 1m from the powder spraying installation and arranged so that powder cannot accumulate or be spilled near to the oven,its air intakes,hot surfaces or any electrical apparatus.Air movement within the oven should not be so high as to blow off powder from the work piece before fusion . The clean air change requirement of the oven should be known and visibly marked on the oven. For conveyor ovens and especially those usingRead More …
How silver ions works in antimicrobial powder coating
Antimicrobial powder coating is widely used in many industries nowadays,such as Building Products,Food Service,Healthcare,Home Products and Packaging.This kind powders contain a silver ions,which act as antagonist over many bacterium. With the presence of moisture, silver ions are gradually released to function as an anti-microbial material. Silver ions charged with plus are drawn toward the microbe’s cell wall charged with minus to disturb the electrical balance. The cell wall of the microbe thus bursts and is extinguished. As silver ions enterRead More …
Requirements for powder coating over hot dip galvanizing
The following specification is recommended: Use zinc phosphate pretreatment if highest adhesion is required. Surface must be perfectly clean. Zinc phosphate has no detergent action and will not remove oil or soil. Use iron phosphate if standard performance is required. Iron phosphate has a slight detergent action and will remove small amounts of surface contamination. Best used for pre-galvanized products. Pre-heat work prior to powder application. Use ‘degassing’ grade polyester powder coating only . Check for correct curing by solventRead More …
The solutions for the problems of powder coating over hot dip galvanizing
1. Incomplete curing: Polyester powder coating powder is thermosetting resins that cross-link to their final organic form by being maintained at a temperature (typically 180 o C), for about 10 minutes. Curing ovens are designed to provide this time at temperature combination. With hot dip galvanized items, with their heavier section thickness, it is necessary to ensure that sufficient stoving time is allowed to meet the curing specifications. Pre-heating of the heavier work will assist in accelerating the curing processRead More …
The problems with powder coating application over galvanized surface
Polyester powder coating over hot dip galvanized steel provides a high grade architectural finish to steel items with excellent atmospheric weathering characteristics.The powder coated product ensures maximum durability for steel components, which will generally provide 50 year+ rust free life spans in most architectural applications. Even so there are still some problems during this application. Hot dip galvanized surfaces have been acknowledged as difficult to powder coating since the technology was first developed in the 1960’s. Industrial Galvanizers commenced research inRead More …
How to prevent powder dust explosion
An explosion can be prevented if both or either of the conditions Explosive Limit and Source of ignition are avoided. Powder coating system should be designed to prevent both conditions occurring ,but due to the difficulty of totally eliminating sources of ignition,more reliance should be placed on the prevention of explosive concentrations of powder. This can be achieved by ensuring that the powder in air concentration is kept below 50% of the Lower Explosive Limit(LEL). Determined LELs on the range ofRead More …
The causes of dust explosion and fire hazards during manufacturing powder coating
Powder coatings are of the fine organic materials, they can give rise to dust explosions. A dust explosion may break out when the following conditions happen at the same time. A ignition sources is present, including: (a) hot surfaces or flames;(b) electrical discharges or sparks;(c) electrostatic discharges. The concentration of dust in the air is between the Lower Explosive Limit (LEL) and Upper Explosion Limit (UEL). when a layer of deposited powder coating or a cloud comes into contact with anRead More …
More superioritis to liquid coating
For many reasons including environmental speaking,excellent performance ,high productivity and economics application,powder coatings have been used more and more since the 1970’s. It is clean,almost zero VOC. Additionally powder coatings provide easy clean up without harmful solvents and harmful waste. Over-sprayed powder can be recycled and reclaimed for greater economic savings than liquids paint.It reduce the cost of labor to coat products as much of application is automated.Powder coatings can not be modified at the clients site,thus eliminating inconsistency of products.Read More …